Repairing small cracks and bumps

Answer:
First sand the surface with sandpaper number 80 until the scratch is no longer visible. Use a wear pad so that the surface remains even.

Sand the surface with sandpaper number 240 or 320 (use water for a smoother surface).



All stones for the same wood-burning stove can be sanded with sandpaper number 320 so that the surface remains even.